Welcome to Baoji Baoye Titanium-Nickel Industry Co., Ltd

The Requirements of Pressure Vessel in Nonferrous Metals especially in Titanium and Nickel

Requiements of Ti/Ni Pressure Vessel


Compression of titanium pressure vessel manufacturing components, shall meet the following requirements
1. Design temperature: pure titanium should not higher than 230 ℃, titanium alloy should not higher than 300 ℃, titanium/Steel clad plate should not be higher than 350 ℃.
2. Pressure vessel shell of titanium material should be used in the annealed state.
3. Titanium pressure vessel head forming hot forming or hot after cold forming to straighten. For forming of titanium steel clad plate head, ultrasonic testing should be done.
4. Titanium pressure vessel is generally not required heat treatment, the use of titanium in stress corrosion environment in the container or use titanium plate made of container, or hot working after welding shall be carried out after eliminating stress annealing. Titanium steel clad plate after explosion compound, eliminate stress annealing treatment should be done.
5. Titanium pressure vessel weld penetration test should be:
(1) Nozzle, flange, reinforcing ring and shell or head connection fillet weld;
(2) Heat exchanger tube and plate connected to the pipe weld;
(3) Titanium steel clad plate cladding weld and fillet cover plate with composite panels lap weld cladding.
Nickel material manufacture pressure vessel pressure parts, shall meet the following requirements:
1. The design temperature, in the annealing state of pure nickel material should not be higher than 650 ℃, nickel copper alloy should not be higher than 480 ℃, Ni - Cr - iron alloy should not be higher than 650 ℃, nickel - iron - chromium alloy should not be higher than 900 ℃.
2. Mainly used in the manufacture of pressure vessel pressure parts of nickel material should be used in annealing state, heat exchanger with linear nickel pipe should be used in eliminating stress annealing conditions.
3. The nickel material head of pressure vessel using hot forming should be strictly control heating temperature. For forming nickel steel composite panels, ultrasonic testing should be done.
4. Hot forming nickel material of heating temperature and heating and heating furnace atmosphere shall be strictly controlled, prevent pollution of sulfur brittleness. Recommend hot working temperature range is:
(1) Pure nickel (N6-2.5-1, 5) is 280 ~ 350 ℃;
(2) Monel (NCU28-2.5-1.5) for 350 ~ 500 ℃;
(3) Inconel (NS312) is 470 ~ 550 ℃;
(4) Hastelloy (NS334) is 930 ~ 1200 ℃.
Nickel material of the pressure vessel magnetic particle or liquid penetrant welds shall be of the following:
(1) Nozzle, flange, reinforcing ring and shell or head connection fillet weld;
(2) Heat exchanger tube plate connected to the pipe weld;
(3) Nickel steel composite board of cladding welding joint.


主站蜘蛛池模板: 国产成人免费在线视频 | 国产福利在线观看精品 | 成年女人a毛片免费视频 | 免费国产一区二区在免费观看 | 欧美成人免费在线观看 | 国内精品视频免费观看 | 国产成人综合日韩精品无 | 久爱www成人网免费视频 | 国产一区二区三区不卡免费观看 | 天天干夜夜 | 波多野吉衣一区二区三区四区 | 久热网| 亚洲你懂的 | 国产欧美一区二区三区免费看 | 特黄特黄一级高清免费大片 | 一级毛片a免费播放王色 | 日日摸日日添夜夜爽97 | 国产精品亚洲综合色区韩国 | 亚洲成人免费看 | 伊人色院成人蜜桃视频 | 国产一区二区在线视频观看 | 一级片成人 | 婷婷色六月 | 亚洲毛片免费在线观看 | 精品国产一区二区三区香蕉事 | 日本一极毛片兔费看 | oldwoman中国老女人tv | 日韩一级黄色大片 | 免费a级毛片出奶水 | 国产成人精品午夜在线播放 | 中文字幕亚洲综合久久菠萝蜜 | 色九九视频 | 久久久午夜 | 国产首页精品 | 全黄h全肉边做边吃奶在线观看 | 色综合久久久久综合体桃花网 | 91九色视频在线观看 | 国产精品麻豆久久99 | 中文字幕 二区 三区 搜查官 | 草久久免费视频 | 久草在线视频免费播放 |